Oxidation of Zr(2) Al(Si) (4)C(5) and Zr(3) Al(Si) (4)C(6) in air

Journal of Materials Research

The oxidation behavior of Zr(2)[Al(Si)](4)C(5) and Zr(3)[Al(Si)](4)C(6) in air has been investigated. The oxidation kinetics of bulk Zr(2)[Al(Si)](4)C(5) and Zr(3)[Al(Si)](4)C(6) at 900-1300 degrees C generally follow a parabolic law at a very short initial stage and then a linear law for a long period with the activation energy of 237.9 and 226.8 kJ/mol, respectively. The oxide scales have a duplex structure, consisting of mainly an outer porous layer of ZrO(2), Al(2)O(3), and aluminosilicate/mullite, and a thin inner compact layer of these oxides plus remaining carbon. The oxidation resistance of Zr(2)[Al(Si)](4)C(5) and Zr(3)[Al(Si)](4)C(6) has been improved compared with Zr(2)Al(3)C(4), and is much better than Zr(3)[Al(Si)](4)C(6) to larger fraction of protective oxidation products, Al(2)O(3) and aluminosilicate/mullite.

关键词: single-crystals;thermoelectric properties;zrc/zro2 interface;zirconium carbide;high-temperatures;bulk zr2al3c4;carbon;mullite;microstructure;ceramics

出版年份

刊物分类

相关作者

相关热词